Field engineer holding a shiny, lightly pitted mild steel corrosion coupon beside a coupon rack at a refinery cooling tower
CASE STUDY · DOWNSTREAM REFINING · COOLING TOWER CORROSION

The program looked excellent, and the coupons were shiny. Mild steel was pitting at 52 mpy.

~$2.1M/yr protected · Pitting eliminated · Relationship intact
~$2.1M/yr
Value protected a year
52 → 0
Mild steel pitting, mpy
<1 mpy
Mild steel general corrosion
334%
Dispersant fed vs. needed

What this case study covers

A refinery cooling tower ran an alkaline phosphate program designed by an account manager who later moved to the customer side and managed the treatment contract. He believed the program was excellent. The coupons were shiny, but mild steel was pitting at 52 mpy, and the contract was up for review. The fix had to work technically without hurting the relationship.

Inside this case study

← Back to Refinery Polymer Overfeed Case Study
📄

Download the Full Case Study

Free · PDF · No spam

✅

Your download is ready

Thank you. Click the button below to download the full case study PDF.

Download PDF

Jim may also be in touch — feel free to reply directly with any questions.

🔒 No spam · Independent advisory · No chemistry sold

Independent · Vendor-Neutral

Have a similar challenge at your facility?

Most assessments begin with a remote review. No vendor pitch — just engineering.

Schedule a Discovery Call